TripleHard mining

      • Comprasionwith Cr6 and TripleHard

      • Cr6: Base material AISI 329 and 20MnV6

      • TripleHard 20MnV6 normal steel

      • Very demandingenvironment in Australianmining

      • Salt and hightemperature

     

     

    20MnV6 + Cr6

      • After 2 months

      • 20MnV6 base material

      • Easy to see a lot of rust

    Need to change the cylinder

     

     

     

     

    AISI329 + Cr6

      • After 4 months

      • AISIbase material

      • Easy to see rust

    Even stainlesssteelrod is rusty

     

     

     

    TripleHard 20MnV6 normal steel

      • After 34 months

      • Normal steel base material

      • NO RUST

    TripleHardis much better than Cr6 with AISI base material